DSpace Repository

Low Temperature Deposition of Lithium Cobalt Oxide for Stable Performance as the Cathode of Solid-State Thin Film Batteries

Show simple item record

dc.contributor.author Bharathi, M. S. D.
dc.contributor.author Raman, K. H. T.
dc.contributor.author Kumar, K. P.
dc.contributor.author Prasanna, S.
dc.contributor.author Rao, G. M.
dc.contributor.author Balasundaraprabhu, R.
dc.date.accessioned 2021-04-11T09:37:02Z
dc.date.accessioned 2022-07-07T05:03:15Z
dc.date.available 2021-04-11T09:37:02Z
dc.date.available 2022-07-07T05:03:15Z
dc.date.issued 2019
dc.identifier.issn 0925-3467
dc.identifier.uri http://repo.lib.jfn.ac.lk/ujrr/handle/123456789/2327
dc.description.abstract There has been a considerable amount of work on the deposition of lithium cobalt oxide thin films on the metalized silicon substrate using room temperature deposition and post-deposition annealing at 700 oC. High-temperature annealing leads to tensile stress-induced cracking in the lithium cobalt oxide thin film. After film cracking, a considerable amount of tensile stress gets stored in the cathode material, that leads to further degradation during the charge-discharge process. The other issue with high-temperature annealing is, lithium desorption that leads to the reduction in the lithium content in the cathode materials. To address this issue, we have developed a deposition process at a lower temperature of 500oC. The substrate used in the process was aluminium and the reason for choosing aluminium was its widely used current collector property in lithium-ion battery fabrication process. The deposited films at 500oC showed predominantly (104) orientation, which is a favourable texture for high diffusivity of lithium. SEM micrographs showed columnar growth and different textures for the films which were deposited with different thicknesses. The Raman spectra showed single phase lithium cobalt oxide and high crystalline nature. To avoid temperature induced effects, magnetron efficiency was also monitored during 500oC substrate temperature. The ideal target to substrate distance was optimized as 6 cm and the sputtering magnetron efficiency was unchanged. The electrochemical performance was evaluated using chronopotentiometry technique and the capacity of the deposited lithium cobalt oxide film was 120 μAh/cm2. The performance of the cathode was stable even up to 80 cycles. en_US
dc.language.iso en en_US
dc.publisher University of Jaffna en_US
dc.title Low Temperature Deposition of Lithium Cobalt Oxide for Stable Performance as the Cathode of Solid-State Thin Film Batteries en_US
dc.type Article en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record