dc.contributor.author Thenmolie, G.
dc.contributor.author Sutharsini, U.
dc.contributor.author Thanihaichelvan, M.
dc.date.accessioned 2024-06-04T05:16:16Z
dc.date.available 2024-06-04T05:16:16Z
dc.date.issued 2018
dc.identifier.uri http://repo.lib.jfn.ac.lk/ujrr/handle/123456789/10594
dc.description.abstract In this study, we investigated the effect of sintering atmosphere and temperature on surface yttria concentration of 3 mole % yttria stabilized tetragonal zirconia polycrystalline (3Y- TZP) ceramic. The 3Y-TZP ceramic powder was die pressed into discs (20mm diameter and 5 mm thickness) followed by cold isostatic pressing at 200 MPa. Then the green compacts were sintered by using tube furnace at air and argon gas atmosphere at sintering temperatures of 1400 ᵒC and 1500 ᵒC for 2 hours. Yttria concentration was measured by X- ray florescent analytical microscope (XRF). The elemental composition was analyzed at twenty different places of the sample using 20 kV, 30 kV and 50 kV as the X-ray tube voltage. Hydrothermal ageing test was conducted in an autoclave containing superheated water steam at 180 ℃ and 10 bar for 12 hours to evaluate the aging resistance of the 3Y-TZP ceramics. That ageing induced tetragonal to monoclinic phase transformation was calculated by using XRD. Studies shows that, average yttria concentration increased with increasing X-ray tube voltage. Thus, the yttria concentration of the sintered sample is increased from surface to interior. On the other hand, surface yttria concentration decreased with increasing sintering temperature from 1400 to 1500 ᵒC. However, sintering atmosphere has a relatively weak influence on the surface yttria concentration. The ageing studies revealed that the ageing is strongly depend on sintering temperature. Sample sintered at 1500 ℃ at air and argon atmosphere more susceptible to hydrothermal ageing. But sample sintered at 1400 ℃ at argon atmosphere shows better hydrothermal ageing compared to other samples. en_US
dc.language.iso en en_US
dc.publisher University of Jaffna en_US
dc.subject 3Y-TZP en_US
dc.subject Zirconia ceramics en_US
dc.subject Aging, XRF en_US
dc.subject Sintering en_US
dc.title Effect of Sintering on Yttria Distribution and Low Temperature Degradation of 3Y-TZP Ceramics en_US
dc.type Article en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record